Country
Full text data for US and EP
Status
Type
Filing Date
Publication Date
Inventor
Assignee
Click to expand
IPC
No.
Publication Number
Title
Publication/Patent Number Publication/Patent Number
Publication date Publication date
Application number Application number
Filing date Filing date
Inventor Inventor
Assignee Assignee
IPC IPC
1
EP1908083A4
Publication/Patent Number: EP1908083A4
Publication date: 2016-07-13
Application number: 06786016
Filing date: 2006-06-30
2
JP5911930B2
Publication/Patent Number: JP5911930B2
Publication date: 2016-04-27
Application number: 2014182373
Filing date: 2014-09-08
Abstract: PROBLEM TO BE SOLVED: To provide a method for making a soft magnetic metal electromagnetic component whose electrical efficiency is improved
3
KR101671048B1
Publication/Patent Number: KR101671048B1
Publication date: 2016-10-31
Application number: 20127007574
Filing date: 2010-08-25
Abstract: 자속 집중기 및 자속 집중기의 제조방법이 제공된다. 본 제조 방법은 연자성체 분말
4
US8984742B2
Publication/Patent Number: US8984742B2
Publication date: 2015-03-24
Application number: 12/217,672
Filing date: 2008-07-08
Abstract: A three dimensional soft magnetic metal mass suitable for milling is formed wrapping soft magnetic metal ribbon into a three dimensional shape and then applying adhesive to the three dimensional shape. The adhesive permeates the three dimensional shape. The adhesive is then cured. If the soft magnetic metal mass is made as a toroid, then it could be processed into an electromechanical component. The electro-mechanical component would then be suitable for use in very high frequency electric motors. A three dimensional soft magnetic metal mass suitable for milling is formed wrapping soft magnetic metal ribbon into a three dimensional shape and then applying adhesive to the three dimensional shape. The adhesive permeates the three dimensional shape. The adhesive is then ...more ...less
5
JP2015047065A
Publication/Patent Number: JP2015047065A
Publication date: 2015-03-12
Application number: 2014182373
Filing date: 2014-09-08
Abstract: PROBLEM TO BE SOLVED: To provide a method for making a soft magnetic metal electromagnetic component whose electrical efficiency is improved
6
CN102598168B
Publication/Patent Number: CN102598168B
Publication date: 2015-06-17
Application number: 201080049434
Filing date: 2010-08-25
Abstract: A flux concentrator and method for manufacturing a flux concentrator is provided. The method can include combining powdered soft magnetic material
7
US8692639B2
Publication/Patent Number: US8692639B2
Publication date: 2014-04-08
Application number: 12/868,052
Filing date: 2010-08-25
Abstract: A flux concentrator and method for manufacturing a flux concentrator is provided. The method can include combining powdered soft magnetic material, a binder, a solvent, a internal lubricant; mixing the materials to create a mixture, evaporating the solvent from the mixture, molding the mixture to form a flux concentrator, and curing the flux concentrator. The flux concentrator may be laminated and broken into multiple pieces, which makes the flux concentrator more flexible. Breaking the flux concentrator does not significantly affect the magnetic properties. Since the permeability of the binder is very similar to that of air, adding tiny air gaps between the fractions is not significantly different than adding more binder. A flux concentrator and method for manufacturing a flux concentrator is provided. The method can include combining powdered soft magnetic material, a binder, a solvent, a internal lubricant; mixing the materials to create a mixture, evaporating the solvent from the mixture ...more ...less
8
TWI451458B
Publication/Patent Number: TWI451458B
Publication date: 2014-09-01
Application number: 99128406
Filing date: 2010-08-25
Abstract: A flux concentrator and method for manufacturing a flux concentrator is provided. The method can include combining powdered soft magnetic material
9
JP2012186999A
Publication/Patent Number: JP2012186999A
Publication date: 2012-09-27
Application number: 2012120593
Filing date: 2012-05-28
Abstract: PROBLEM TO BE SOLVED: To enable a formed electromechanical component to have attractive soft magnetic properties
10
KR20120057636A
Publication/Patent Number: KR20120057636A
Publication date: 2012-06-05
Application number: 20127007574
Filing date: 2010-08-25
Abstract: 자속 집중기 및 자속 집중기의 제조방법이 제공된다. 본 제조 방법은 연자성체 분말
11
CN102598168A
Publication/Patent Number: CN102598168A
Publication date: 2012-07-18
Application number: 201080049434
Filing date: 2010-08-25
Abstract: A flux concentrator and method for manufacturing a flux concentrator is provided. The method can include combining powdered soft magnetic material
12
CN1839451B
Publication/Patent Number: CN1839451B
Publication date: 2011-05-25
Application number: 200480023218
Filing date: 2004-06-02
Abstract: The invention provides a method for producing a three dimensional soft magnetic metal electro-mechanical component
13
AU2006265907B2
Publication/Patent Number: AU2006265907B2
Publication date: 2011-02-17
Application number: 2006265907
Filing date: 2006-06-30
14
WO2011031473A2
Publication/Patent Number: WO2011031473A2
Publication date: 2011-03-17
Application number: 2010046611
Filing date: 2010-08-25
Abstract: A flux concentrator and method for manufacturing a flux concentrator is provided. The method can include combining powdered soft magnetic material
15
US20110050382A1
Publication/Patent Number: US20110050382A1
Publication date: 2011-03-03
Application number: 12/868,052
Filing date: 2010-08-25
Abstract: A flux concentrator and method for manufacturing a flux concentrator is provided. The method can include combining powdered soft magnetic material, a binder, a solvent, a internal lubricant; mixing the materials to create a mixture, evaporating the solvent from the mixture, molding the mixture to form a flux concentrator, and curing the flux concentrator. The flux concentrator may be laminated and broken into multiple pieces, which makes the flux concentrator more flexible. Breaking the flux concentrator does not significantly affect the magnetic properties. Since the permeability of the binder is very similar to that of air, adding tiny air gaps between the fractions is not significantly different than adding more binder. A flux concentrator and method for manufacturing a flux concentrator is provided. The method can include combining powdered soft magnetic material, a binder, a solvent, a internal lubricant; mixing the materials to create a mixture, evaporating the solvent from the mixture ...more ...less
16
TW201126551A
Publication/Patent Number: TW201126551A
Publication date: 2011-08-01
Application number: 99128406
Filing date: 2010-08-25
Abstract: A flux concentrator and method for manufacturing a flux concentrator is provided. The method can include combining powdered soft magnetic material
17
WO2011031473A3
Publication/Patent Number: WO2011031473A3
Publication date: 2011-06-23
Application number: 2010046611
Filing date: 2010-08-25
Abstract: A flux concentrator and method for manufacturing a flux concentrator is provided. The method can include combining powdered soft magnetic material
18
AU2004246416B2
Publication/Patent Number: AU2004246416B2
Publication date: 2010-08-26
Application number: 2004246416
Filing date: 2004-06-02
19
CA2529200C
Publication/Patent Number: CA2529200C
Publication date: 2010-11-09
Application number: 2529200
Filing date: 2004-06-02
Abstract: A three dimensional soft magnetic metal mass suitable for milling is formed wrapping soft magnetic metal ribbon (10) into a three dimensional shape and then applying adhesive to the three dimensional shape. The adhesive permeates the three dimensional shape. The adhesive is then cured. If the soft magnetic metal mass is made as a toroid (18) A three dimensional soft magnetic metal mass suitable for milling is formed wrapping soft magnetic metal ribbon (10) into a three dimensional shape and then applying adhesive to the three dimensional shape. The adhesive permeates the three dimensional shape. The adhesive is then ...more ...less
20
US20090032141A1
Publication/Patent Number: US20090032141A1
Publication date: 2009-02-05
Application number: 12/217,672
Filing date: 2008-07-08
Abstract: A three dimensional soft magnetic metal mass suitable for milling is formed wrapping soft magnetic metal ribbon into a three dimensional shape and then applying adhesive to the three dimensional shape. The adhesive permeates the three dimensional shape. The adhesive is then cured. If the soft magnetic metal mass is made as a toroid, then it could be processed into an electromechanical component. The electromechanical component would then be suitable for use in very high frequency electric motors. A three dimensional soft magnetic metal mass suitable for milling is formed wrapping soft magnetic metal ribbon into a three dimensional shape and then applying adhesive to the three dimensional shape. The adhesive permeates the three dimensional shape. The adhesive is then ...more ...less